BOMBA LA CHUMA LA KABONI BOMBA LA CARBON ISO LILILO NA MFUMO BOMBA LA CHUMA LA KABONI BOMBA LISILO NA MFUMO
Maelezo
Bomba la Chuma lisilo na mshono limetengenezwa kutoka kwa chuma kigumu cha duara 'billet' ambacho hupashwa moto na kusukumwa au kuvutwa juu ya umbo hadi chuma hicho kitengenezwe kuwa bomba tupu.Bomba lisilo na mshono hukamilishwa kwa vipimo vya dimensional na unene wa ukuta kwa ukubwa kutoka inchi 1/8 hadi inchi 32 OD.Carbon Steel Imefumwa Mabomba / Mirija Chuma cha kaboni ni aloi inayojumuisha chuma na kaboni.Asilimia ya kaboni katika chuma huathiri ugumu, nguvu ya elasticity na ductility ya chuma kaboni.Bomba la chuma cha kaboni isiyo imefumwa au ingot ya chuma imara hufanywa kwa tube ya capillary kupitia shimo, kisha kwa njia ya simu ya moto-iliyovingirishwa, baridi au baridi hufanywa.Imefumwa kaboni chuma bomba katika sekta ya China chuma ina nafasi muhimu.Nyenzo za bomba la chuma cha kaboni isiyo imefumwa ni mirija ya duara, viinitete vya mashine ya kukata bomba kupitia kukata kwa urefu wa mita 1 bila kitu, na kutumwa na kupokanzwa tanuru ya ukanda wa conveyor.Billet inalishwa ndani ya tanuru ya joto, joto ni karibu digrii 1200 Celsius.Mafuta ni hidrojeni au asetilini.Udhibiti wa joto la tanuru ni suala kuu.Bomba la pande zote lilitoka ili kupiga mashine kupitia shinikizo la hewa.Ujumla zaidi ya kawaida ngumi ni tapered roll utoboaji mashine, Punch high uzalishaji ufanisi, ubora wa bidhaa, kubwa kipenyo shimo upanuzi, wanaweza kuvaa aina ya chuma.Utoboaji, bomba la pande zote limekuwa kwenye rolling tatu, rolling au extrusion.Imebanwa kutoka kwa bomba baada ya ukubwa.Kupima kwa koni ya mzunguko wa kasi toboa mashimo kwenye billet ili kuunda mirija.Kipenyo cha bomba kwa kinu cha kupima ili kuamua urefu wa kipenyo cha kuchimba.Baada ya bomba kupitia sizing ndani ya mnara wa baridi, baridi kwa dawa ya maji, chuma baada ya baridi, lazima straightening.Baada ya ukanda wa chuma uliotumwa na kunyoosha mashine ya kupima chuma (au mtihani wa shinikizo) kwa kupima ndani.Ikiwa bomba hupasuka ndani, Bubbles na matatizo mengine yatagunduliwa.Baada ya bomba lakini pia kwa njia ya kali kudhibiti ubora wa uteuzi mwongozo.Ubora wa chuma, matumizi ya nambari za rangi ya dawa, vipimo, nambari ya kura ya uzalishaji.Kwa crane ndani ya ghala.
Unene wa ukuta wa bomba isiyo imefumwa
Uvumilivu wa Kipenyo cha Nje na unene wa Ukuta
Vipimo
Kawaida | Maelezo |
ASTM A179/A179M | Kibadilisha joto cha chuma cha aloi ya chini imefumwa na mirija ya condenser. |
API 5L | Bomba la mstari. |
ASTM A53M | Bomba la Chuma Nyeusi na Zinki Lililopakwa kwa Welded na Imefumwa. |
ASTM A106M | Bomba la chuma cha kaboni isiyo imefumwa kwa huduma ya joto la juu. |
ASTM A105M | Ughushi wa chuma cha kaboni kwa matumizi ya bomba. |
ASTM A234M | Uwekaji wa mabomba ya chuma cha kaboni na aloi ya chuma kwa ajili ya huduma ya joto la wastani na la juu. |
Kawaida
Kawaida | Aina ya bomba | Darasa | Daraja |
API SPEC 5L ISO 3183 | SMLS | PLS1 | L245B, L290 X42, L320 X46 , L360 X52, L390 X56, L415 X60, L450 X65, L485 X70 |
PLS2 | L245N BN, L290N X42N, L320N X46N, L360N X52N, L390N X56N, L415N X60N, L360Q X52Q, L390Q X56Q, L415Q X60Q , L485Q X70Q | ||
Mazingira Machafu ya PLS2 | L245NS BNS, L290NS X42NS, L320NS X46NS L360NS X52NS, L390NS X56NS, L415NS X60NS, L360QS X52QS, L390QS X56QS, L415QS X60QS L485QS X70QS | ||
WELD | PLS1 | L245B, L290 X42, L320 X46, L360 X52 L390 X56, L415 X60, L450 X65, L485 X70 | |
PLS2 | L245M BM, L290M X42M, L320M X46M, L360M X52M, L390M X56M, L415M X60M, L450M X65M, L485M X70M, L555M X80M, |
Kawaida | Daraja |
ASTM A 53 M | A, B |
ASTM A 106M | A, B, C |
JIS G 3454 | STPG 370, STPG 410 |
JIS G 3455 | STPG370, STPG410, STPG480 |
JIS G 3456 | STPG370, STPG410, STPG480 |
Daraja: Muundo wa Kemikali (%):
Kawaida | Daraja | C | Si | Mn | P | S | Ni | Cr | Cu | Mo | V |
ASTMA 53M | A | ≤0.25 | - | ≤0.95 | ≤0.05 | ≤0.045 | ≤0.40 | ≤0.40 | ≤0.40 | ≤0.15 | ≤0.08 |
B | ≤0.30 | - | ≤1.20 | ≤0.05 | ≤0.045 | ≤0.40 | ≤0.40 | ≤0.40 | ≤0.15 | ≤0.08 | |
ASTM A 106M | A | ≤0.25 | ≥0.10 | 0.27-0.93 | ≤0.035 | ≤0.035 | ≤0.40 | ≤0.40 | ≤0.40 | ≤0.15 | ≤0.08 |
B | ≤0.30 | ≥0.10 | 0.29-1.06 | ≤0.035 | ≤0.035 | ≤0.40 | ≤0.40 | ≤0.40 | ≤0.15 | ≤0.08 | |
C | ≤0.35 | ≥0.10 | 0.29-1.06 | ≤0.035 | ≤0.035 | ≤0.40 | ≤0.40 | ≤0.40 | ≤0.15 | ≤0.08 | |
JIS G 3454 | STPG 370 | ≤0.25 | ≤0.35 | 0.30-0.90 | ≤0.040 | ≤0.040 | - | - | - | - | - |
STPG 410 | ≤0.30 | ≤0.35 | 0.30-1.00 | ≤0.040 | ≤0.040 | - | - | - | - | - | |
JIS G 3455 | STS 370 | ≤0.25 | 0.10-0.35 | 0.30-1.10 | ≤0.035 | ≤0.035 | - | - | - | - | - |
STS 410 | ≤0.30 | 0.10-0.35 | 0.30-1.40 | ≤0.035 | ≤0.035 | - | - | - | - | - | |
STS 480 | ≤0.33 | 0.10-0.35 | 0.30-1.50 | ≤0.035 | ≤0.035 | - | - | - | - | - | |
JIS G 3456 | STPT 370 | ≤0.25 | 0.10-0.35 | 0.30-0.90 | ≤0.035 | ≤0.035 | - | - | - | - | - |
STPT 410 | ≤0.30 | 0.10-0.35 | 0.30-1.00 | ≤0.035 | ≤0.035 | - | - | - | - | - | |
STPT 480 | ≤0.33 | 0.10-0.35 | 0.30-1.00 | ≤0.035 | ≤0.035 | - | - | - | - | - |
Uchoraji & Kupaka
Matibabu ya uso wa bomba la chuma: Ili kuboresha maisha ya huduma ya bomba la mafuta, matibabu ya uso kwa kawaida hufanywa ili kuwezesha mchanganyiko thabiti wa bomba la chuma na mipako ya kuzuia kutu. Mbinu za kawaida za usindikaji ni: kusafisha, kuondoa chombo, kuokota, ulipuaji wa risasi. makundi manne.
1.Kusafisha Grisi, vumbi, lubricant, suala la kikaboni kuzingatiwa juu ya uso wa bomba la chuma, kwa kawaida kwa kutumia kutengenezea, emulsion kusafisha uso.Hata hivyo, kutu, ngozi ya oksidi na slag ya kulehemu kwenye uso wa bomba la chuma haiwezi kuondolewa; kwa hivyo mbinu zingine za matibabu zinahitajika. Uondoaji kutu wa Zana Oksidi ya uso wa bomba la chuma, kutu, slag ya kulehemu, inaweza kutumia brashi ya waya ya chuma kusafisha na kung'arisha uso wa uso.
2. Uharibifu wa zana unaweza kugawanywa katika mwongozo na nguvu, uharibifu wa chombo cha mwongozo unaweza kufikia kiwango cha Sa 2, uharibifu wa chombo cha nguvu unaweza kufikia kiwango cha Sa3. Ikiwa uso wa bomba la chuma umeunganishwa na ngozi yenye nguvu ya oksidi, inaweza kuwa vigumu kuiondoa. kutu kwa msaada wa zana, hivyo tunahitaji kutafuta njia nyingine.
3.Kuchuna Njia za kawaida za kuchuna ni pamoja na kemia na electrolysis.Lakini uchunaji wa kemikali pekee ndio hutumika kwa ajili ya ulinzi wa kutu wa bomba.Uchunaji wa kemikali unaweza kufikia kiwango fulani cha usafi na ukali kwenye uso wa bomba la chuma, ambalo ni rahisi kwa waya zinazofuata. risasi (mchanga) baada ya kusindika tena.
4.Ulipuaji wa risasi ili kuondoa kutu. Kwa kutumia motor yenye nguvu nyingi endesha blade zinazozunguka za kasi ya juu, grit ya chuma, risasi ya chuma, sehemu, madini na waya nyingine za abrasive chini ya hatua ya nguvu ya kati kwenye mnyunyizio wa uso wa bomba la chuma na utoaji mkubwa, ondoa kikamilifu. kutu, oksidi na uchafu kwa upande mmoja, kwa upande mwingine, bomba la chuma chini ya hatua ya athari kali ya abrasive na nguvu ya msuguano, ili kufikia ukali unaohitajika. Miongoni mwa njia nne za matibabu, ulipuaji wa risasi na uharibifu ni njia bora ya matibabu kwa kupungua kwa bomba.Kwa ujumla, ulipuaji na uondoaji rutuba hutumika zaidi kwa matibabu ya uso wa ndani wa bomba la chuma, na ulipuaji na uondoaji wa risasi hutumiwa zaidi kwa matibabu ya uso wa nje wa bomba la chuma.
Kupakia&Kupakia
Kunyunyizia rangi
Ufungaji wa kuzuia maji